Estilo |
Ancho |
Peso |
Malla |
Resistencia a la ruptura |
porosidad |
Contenido de SiO2 |
Tejer |
|
|
N/25×100 mm |
||||||||
|
Urdimbre |
Trama |
|||||||
|
BNT1.5×1.5-83 |
83 ± 3 |
135 ± 14 |
1,5 × 1,5 |
≥90 |
≥80 |
55 |
≥96 |
gasa de lino |
|
BNT2×2-83 |
83 ± 3 |
125 ± 13 |
2,0 × 2,0 |
≥85 |
≥70 |
65 |
≥96 |
gasa de lino |
|
BNT2.5×2.5-83 |
83 ± 3 |
110 ± 11 |
2,5 × 2,5 |
≥68 |
≥62 |
70 |
≥96 |
gasa de lino |
|
BNT1.5×1.5-83 M |
83 ± 3 |
380 ± 38 |
1,5 × 1,5 |
≥300 |
≥250 |
19 |
≥96 |
Imitación de gasa de vuelta |
|
BNT2×2-83 M |
83 ± 3 |
350 ± 35 |
2,0 × 2,0 |
≥250 |
≥200 |
24 |
≥96 |
Imitación de gasa de vuelta |
|
BNT2.5×2.5-83 M |
83 ± 3 |
310 ± 31 |
2,5 × 2,5 |
≥200 |
≥150 |
33 |
≥96 |
Leno simulado |